For equipment and valve parts manufacturers, the main issue they are facing is SCC(tress Corrosion Cracking) which intends to generate in sulfur containing oil wells.
As a material vendor, ECA hopes to address it.
We find the cooling method makes a difference to Alloy 718’s hardness, surface residual stress and grain boundaries.
The popular cooling method is water cool in most mills as it is economical and time-saving. ECA finds the water quenching refines the grain size and increase the tensile strength of the material, but γ″phases precipitated amounts get expanded and residual stress on the material surface increase at the same time, following HE(Hydrogen embrittlement) susceptibility and micro-cracks for thick walled valve parts.
In the contrast, ECA tries to work with our partner mills to try water cooling.We found continuous acicular δ phase is suppressed and the hardness 34–40 HRC is more controllable compared to water cooling leading to a reduced possibility of SSC(Sulfide stress cracking) and SCC (Stress corrosion cracking).
The micrograph of Alloy 718 with water cooling illustrates it.

Do you have quality concerns when importing Chinese Alloy 718 material for oil & gas application?
What is the difference between API 6A CRA, AMS 5662 and AMS 5663? All three standards define material requirements for Alloy 718. AMS 5662 and AMS 5663 cover Alloy 718 for aerospace engine service, not imposing mandatory requirements for sour-service resistance, transverse Charpy impact. AMS 5662 specifies Alloy 718 supplied in the solution-annealed condition, whereas AMS 5663 covers material delivered in the solution-annealed and age-hardened condition. API 6A CRA governs Alloy 718 for sour-service oil and gas wellhead applications. It is tailored for pressure-containing and pressure-controlling components used on wellheads and Christmas trees under sour oil and gas service (H₂S, Cl⁻), and aligns with NACE MR0175 / ISO 15156.
How does the cooling methods influence Alloy 718 material’ performance in oil & gas sector?
What is the difference between Alloy 718 and Alloy 725?