Industry news
-
Why bubbles appear at the Kovar-glass sealing interface during hermetic sealing?
Interface bubbles are a common failure in Kovar hermetic sealing. The root causes are from carbon control, surface cleanliness and pre-oxidation parameters for glass-to-metal sealing.Read more -
Do you have quality concerns when importing Chinese Alloy 718 material for oil & gas application?
Over a series of case stories, ECA will show you the remarkable progress of China’s alloy 718 material manufacturing.Read more -
What is the difference between API 6A CRA, AMS 5662 and AMS 5663?
API 6A CRA governs Alloy 718 for sour-service oil and gas wellhead applications while AMS 5662 and AMS 5663 cover Alloy 718 for aerospace engine service.Read more -
How does the cooling methods influence Alloy 718 material’ performance in oil & gas sector?
The cooling method after heat treatment makes a difference to Alloy 718’s quality in hardness, surface residual stress and grain boundaries.Read more -
What is the difference between Alloy 718 and Alloy 725?
Alloy 718 and Alloy 725 are both nickel-based precipitation hardening superalloys, yet they differ notably in chemical composition, mechanical performance and application scenarios.Read more